How to solve the friction traces of the glass bottle body

Many users are impressed by the friction traces between glass bottle products. How to solve these problems has long plagued many glass bottle manufacturers. At present, many customers' requirements for product quality are getting higher and higher, and the quality of the original products can no longer meet the needs of the current glass container market.

037.jpg

When the glass bottle factory is installed in the assembly line of the workshop, a thermal spray technology process is added between the route conveyors. The bottle from the formation of the ranking machine can be sprayed. After the glass bottle entered the second annealing of different annealing kilns, the trace of the bottle design will not develop a trace of impact when it develops. After the glass bottle comes out at the conveyor belt of the secondary annealing kiln, the bottle body is still there is just the bottle body. When some remaining temperature, then through a national cold spray construction technology (a special chemical industrial product), so that students will continue to improve my country's country with a secondary spray glass bottle transparency and smoothness. The scratches caused by friction between the glass bottle and the bottle will be alleviated, and it will have a good tougher to enhance the social effect on the glass bottle.


Looking for a supplier of high-quality borosilicate glass kitchenware

Get started today by requesting a free quote.